MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Xtel® XE4050BL Polyphenylene Sulfide Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Xtel® XE4050BL is a glass fiber and mineral filled PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.

Information provided by Chevron Phillips

Measured on 102mm x 102mm x 3.2 mm plaques, edge gated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccISO 1183A
Water Absorption 0.030 %ASTM D-570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 130 MPaISO 527
Elongation at Yield 1.7 %ISO 527
Flexural Strength 190 MPaISO 178
Flexural Modulus 11.0 GPaISO 178
Compressive Strength 195 MPaISO 604
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²ISO 180A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D-257
Dielectric Constant 4.0
@Frequency 1e+6 Hz
ASTM D-150
 4.1
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 20.0 kV/mmASTM D-149
Dissipation Factor 0.0030
@Frequency 1000 Hz
ASTM D-150
 0.0090
@Frequency 1e+6 Hz
ASTM D-150
Arc Resistance 120 secASTM D-495
Comparative Tracking Index 150 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 100 - 200 °C
Axial; ISO 11359-2
 20.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
Axial; ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ISO 11359-2
 100 µm/m-°C
@Temperature 100 - 200 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Melt Temperature 315 - 345 °C
Mold Temperature 135 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced
Barlog Plastics KEBATRON C1040G5 PPS, cross-linked, 40% glass fiber reinforced

PCHEVD259 / 20753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.