MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite Durez® 12687 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez 12687 is a finely pulverized two-step phenolic resin. Durez 12687 is recommended for use as a processing aid and reinforcing resin for NBR (nitrile) rubber.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccDCT 0170
Particle Mesh Size 200 Mesh200 MeshDCT 4007A
 
Thermal PropertiesMetricEnglishComments
Melting Point 75.0 °C167 °FClear; DCT 0011B
 
Processing PropertiesMetricEnglishComments
Cure Time 0.450 min
@Treatment Temp. 165 °C
0.00750 hour
@Treatment Temp. 329 °F
DCT 0162B
 
Descriptive Properties
% Hexamine Content7.4DCT 126B
AppearanceBrown Powder
Inclined Plate Flow; 0.5g, 125°C, mm75DCT 0351C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 12686 Phenolic Novolac
Sumitomo Bakelite Durez® 12687 CNSL Phenolic Resin
Lanxess LEWATIT® MonoPlus TP 260 Cation Exchange Resin
Sumitomo Bakelite Plyophen P23983 Phenolic Resin
Sumitomo Bakelite Plyophen 43703 Phenolic Resin

PSUMIT214 / 194019

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.