MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-97-T0207G-87UV Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TL-97-T0207G-87UV is a high performance flame retardant thermoplastic elastomer designed for electrical applications including fiber optics. It is a high hardness, medium density, UV stabilized grade that is suitable for extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Flame Retardant; Good Adhesion; Good Processability; Good Tear Strength; Good Toughness; High Hardness; Light Stabilized; Low Flow; Medium Density; Slip; Sunlight Resistant; UV Resistant

Uses: Fiber Optic Cable; Industrial Applications; Rubber Replacement

RoHS Compliant:RoHS

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Viscosity 549 cP
@Shear Rate 206 1/s,
Temperature 200 °C
549 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 1.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.2 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  42
@Time 5.00 sec
42
@Time 0.00139 hour
ISO 815
 49
@Time 1.00 sec
49
@Time 0.000278 hour
ISO 815
Tensile Strength at Break 7.79 MPa1130 psiFlow; ISO 37
 10.5 MPa1520 psiAcross Flow; ISO 37
 9.48 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1380 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  5.23 MPa
@Strain 100 %
759 psi
@Strain 100 %
Across Flow; ISO 37
 7.10 MPa
@Strain 100 %
1030 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 370 %370 %Flow; ISO 37
 820 %820 %Across Flow; ISO 37
 775 %
@Treatment Temp. 125 °C,
Time 605000 sec
775 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tear Strength 59.6 kN/m340 pliFlow; ISO 34-1
 61.4 kN/m350 pliAcross Flow; ISO 34-1
Compression Set  49 %
@Temperature 22.8 °C,
Time 79200 sec
49 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 88 %
@Temperature 70.0 °C,
Time 79200 sec
88 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 94 %
@Temperature 90.0 °C,
Time 252000 sec
94 %
@Temperature 194 °F,
Time 70.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -55.0 °C<= -67.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 188 - 210 °C370 - 410 °FInjection, Melt
Rear Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Middle Barrel Temperature 177 - 199 °C350 - 390 °FInjection
Front Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Nozzle Temperature 188 - 210 °C370 - 410 °FInjection
Zone 1 166 - 199 °C330 - 390 °FExtrusion
Zone 2 171 - 204 °C340 - 400 °FExtrusion
Zone 3 177 - 210 °C350 - 410 °FExtrusion
Zone 4 182 - 216 °C360 - 420 °FExtrusion
Zone 5 182 - 216 °C360 - 420 °FExtrusion
Die Temperature 190 - 210 °C374 - 410 °FExtrusion
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1635 / 238126

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.