MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Chemicals Sulphur Hexafluoride Technical Grade
Categories: Fluid

Material Notes: Sulphur Hexafluoride (SF6) is a non-toxic, inert, insulating and cooling gas of high dielectric strength and thermal stability. It is used for electrical engineering and foundry practice.

CAS-No.: 2551-62-4 / EC-No.: 219-854-2 /REACH Registration Number: 01-2119458769-17

Uses: Electrical industry and Metallurgy

Information provided by Solvay

Key Words: Sulfur Hexafluoride, SF6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 146 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point -50.8 °C
Boiling Point -63.8 °CSublimation point
 
Descriptive Properties
Appearancecompressed liquefied gas
Colorcolorless
Composition>99.9%Sulfur hexafluoride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
Sulfur Hexafluoride, SF6
Unipetrol Liquid Sulfur
Telles Mirel™ P1004 Injection Molding Grade PHA Bioplastic
Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic

WSOLV091 / 147740

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.