MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.

Applications: Extrusion on to metal pipes to produce a corrosion resistant coating for buried pipe systems.

Data provided by the manufacturer.

Key Words: High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccASTM D792
ESCR 100% Igepal® >= 1000 hourF50, condition B; ASTM D1693
Melt Flow 0.38 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Break 500 %ASTM D638
Flexural Modulus 0.565 GPaASTM D790
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+17 ohm-cmASTM D257
Surface Resistance 1.00e+17 ohminsulation resistance
Dielectric Constant 2.34ASTM 1531
Dissipation Factor 0.00010ASTM 1531
 
Thermal PropertiesOriginal ValueComments
Melting Point 129 °CASTM D3417
Vicat Softening Point 122 °CASTM D1525
Brittleness Temperature <= -70.0 °CASTM D696
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 230 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 51-35BP HDPE Extrusion Resin
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin
Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin
Chevron Phillips Marlex® K608 HDPE Extrusion Molding Resin
Braskem GP5550BK HDPE High Density Extrusion Polyethylene

PEHN0V / 35544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.