MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Pavprene® 501 Polymeric Bitumen Modifier
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: SO.F.TER. offers the market a range of products capable of meeting every need in the road paving sector. The products are divided into two groups which differ in molecular structure. The linear structure enables to obtain bituminous blends that offer lower viscosity and improved sprayability, processability, emulsionability and storage stability, as well as better compatibility with the different types of bitumen.

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D 792
Volatiles <= 0.70 %ASTM D 5668
Brookfield Viscosity 415 cPBitumen 80/100 + 5 phb of polymer; SO.F.TER.
Viscosity Measure 13 cStin Toluene 5.23%; SO.F.TER. Method
Ash <= 0.40 %ASTM D 5667
 
Chemical PropertiesOriginal ValueComments
Styrene Content 31 %ASTM D 5775
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76ASTM D 2240
Penetration P(0), 1/10 mm 53Bitumen 80/100 + 5 phb of polymer; ASTM D 5
Tensile Set >= 95 %Bitumen 80/100 + 5 phb of polymer; CNR 44
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 80.0 °CBitumen 80/100 + 5 phb of polymer; ASTM D 36
 
Descriptive Properties
Max. Anti-packing Agent (%)1
Min. Ductility (cm)70CNR 44; Bitumen 80/100 + 5 phb of polymer
Physical Aspectcrumbs
Structurelinear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Concrete, 1-4 Dry
Unipetrol 70/100 Road Bitumen
Unipetrol 50/70 Road Bitumen
Unipetrol 160/220 Road Bitumen

PSOFS601 / 162065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.