MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eastman Regalrez™ 3102 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Regalrez™ 3102 hydrocarbon resin is produced by polymerization and partial hydrogenation of pure monomer hydrocarbon feedstocks. It is highly stable, light colored, low molecular weight, nonpolar resin suggested for use in adhesives, coatings, sealants, and caulks. Due to its low color, high stability and balance of cycloaliphatic and aromatic structure, Regalrez™ 3102 provides a bredth of compatibility that is not possible with a purely aromatic or aliphatic resin. It is suggested for use in applications where fully hydrogenated or pure monomer aromatic resins are incompatible or do not give the desired balance of properties.

Application/Uses:

  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Film Modification
  • Hot Melt Adhesives
  • Paint and Coatings
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Wax Modification

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Viscosity 100 cP
@Temperature 195 °C
Melt
 1000 cP
@Temperature 160 °C
Melt
 10000 cP
@Temperature 135 °C
Melt
 100000 cP
@Temperature 125 °C
Melt
Molecular Weight 800 g/molMn
 1500 g/molMw. Mw/Mn ratio = 1.9
 2400 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 50.0 °C
Ring & Ball Softening Point 103 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point<-40°COMSCP
 25°CMMAP
 -29°CDACP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5560 / 222754

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.