A 13% glass fiber reinforced Nylon 6, designed to provide a high flexural modulus and good dimensional stability, while maintaining the ease of processing associated with Nylon 6 type materials. Data provided by the manufacturer |
Polyamide 6; Ashley Polymers, Inc. |