MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 289-IN VRN Mixture of methyl ethyl ketone peroxide and cumyl hydroperoxide, in solvent mixture
Categories: Other Engineering Material

Material Notes: Trigonox 289-IN VRN is a special peroxide blend with a VRN system, suitable for curing unsaturated polyester and vinylester resins at ambient conditions in conjunction with a metal accelerator.

CAS number: 1338-23-4; 80-15-9

EINECS/ELINCS No: 215-661-2; 201-254-7

Applications: Trigonox 289-IN VRN is a convenient initiator suitable for curing unsaturated polyester, vinyl ester and acrylic thermosetting resins at ambient conditions in conjunction with a metal salt. Trigonox 289-IN VRN offers the advantages of a standard red peroxide formulation to indicate product flow and proper mixing into the resin. The vanishing red (VR) series of products however include a red indicator system that disappears during the cure. The red color is only visible when needed but not in the finished end product. The key features are: indicates initiator presence, monitoring of the mixing step, monitoring of the cure by color and indicating under-cured area's in the mould, and last but not least it leaves the end product colorless after the cure.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
Viscosity 23 cP
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceClear red liquid
Content8.8-9.0 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1085 / 286608

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.