Hostacom EKE 787L NATRL medium high melt flow, 2,400 MPa flexural modulus, 40% Calcium Carbonate-filled polypropylene copolymer resin has a very good balance of properties and processability. It is typically used for appliance applications that require good chemical resistance. Applications: Appliances.Information provided by LyondellBasell. |