MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid
Categories: Fluid

Material Notes: Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strongly resist degradation while holding thermal properties and maintaining efficiency. This provides for low mainetance and solid performance over an extended operating life. Non-toxic, the HE fluid is safe to use and easy to dispose. It can be safely combined with spent lubricating oils and recycled locally.

Information provided by Paratherm Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.22 lb/gal
@Temperature 15.6 °C
API Gravity 31.7 °ASTM D287
Kinematic Viscosity at 40°C (104°F) 40.25 cStASTM D445
Molecular Weight 445 g/molaverage; ASTM D2502
Vapor Pressure 0.00002654 atm
@Temperature 149 °C
 0.0001313 atm
@Temperature 177 °C
 0.000660 atm
@Temperature 204 °C
 0.002633 atm
@Temperature 232 °C
 0.009186 atm
@Temperature 260 °C
 0.0263 atm
@Temperature 288 °C
 0.0592 atm
@Temperature 316 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 3.00 kV/mm
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 42.88 cal/gcalculated
CTE, linear 592 µin/in-°F
@Temperature 20.0 °C
Boiling Point 415 °C
@Pressure 0.101 MPa
10% fraction; ASTM D1160
Maximum Service Temperature, Air 600 °Foptimum use range
 <= 650 °Fmax. recommended film temperature
Minimum Service Temperature, Air 150 °Foptimum use range
Pour Point 5.00 °FASTM D97
Flash Point 440 °Fcoc; ASTM D92
Ignition Temperature 700 °FAutoignition; ASTM D2155
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4722ASTM D1747
 
Descriptive Properties
Appearancetransparent, pale yellow
Color1ASTM D1500
Corrosivity1A3hr Cu Strip @ 100°C, ASTM D130
Feedstockparaffinic hydrocarbon
Fire point 500°FASTM D92, coc
Heat of Combustion 19550 BTU/lbASTM D92
Odorfaint (oily)
Pumpability20°Fcentrifugal at 2000 centipoise
Sulfur Content0.002 Mass %J-140
Total Acid Number0.01ASTM D664

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid

WPAR01 / 76876

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.