MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TL-8712R Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Telcar TL-8712R is a flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Telcar TL-8712R is a medium hardness, medium duromenter grade that is RoHS compliant. This grade is suitable for both injection molding and extrusion.

Features: Flame Retardant; General Purpose; Good Colorability; Good Flexibility; Halogenated, Heat Aging Resistant; High Elasticity; High Elongation; High Tensile Strength; Low Flow; Medium Hardness

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Underground Power Cable; Wire and Cable Applications; Wire Jacketing

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171ASTM D2240
Tensile Strength at Break 13.8 MPa2000 psi0.02 in, Die C, 20 in/min, die cut from extruded tapes; ASTM D412
 12.7 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
1840 psi
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 15.04 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
2181 psi
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
Tensile Stress at Strain  2.48 MPa
@Strain 100 %,
Thickness 0.508 mm
360 psi
@Strain 100 %,
Thickness 0.0200 in
Die C, 20 in/min, die cut from extruded tapes; ASTM D412
 3.65 MPa
@Strain 300 %,
Thickness 0.508 mm
530 psi
@Strain 300 %,
Thickness 0.0200 in
Die C, 20 in/min, die cut from extruded tapes; ASTM D412
Elongation at Break 680 %680 %0.02 in, Die C, 20 in/min, die cut from extruded tapes; ASTM D412
 673.2 %
@Treatment Temp. 136 °C,
Time 605000 sec
673.2 %
@Treatment Temp. 277 °F,
Time 168 hour
in Air; ASTM D573
 700.4 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
700.4 %
@Treatment Temp. 140 °F,
Time 168 hour
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.60e+15 ohm-cm
@Temperature 50.0 °C
6.60e+15 ohm-cm
@Temperature 122 °F
ASTM D257
Dielectric Constant  2.1
@Frequency 1000 Hz
2.1
@Frequency 1000 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 26.0 kV/mm660 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FASTM D794
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
Flammability, UL94 HBHB0.12 in, All Colors
Oxygen Index 20 %20 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 193 °C340 - 380 °F
Middle Barrel Temperature 177 - 199 °C350 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 188 - 210 °C370 - 410 °F
Zone 1 166 - 188 °C330 - 370 °F
Zone 2 171 - 193 °C340 - 380 °F
Zone 3 177 - 199 °C350 - 390 °F
Zone 4 188 - 207 °C370 - 405 °F
Zone 5 182 - 204 °C360 - 400 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 188 - 210 °C370 - 410 °FProcessing Temperature
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis PC0787 Polyethylene Insulation Compound, Crosslinkable
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
Borealis Polycure™ PC780 Flame Retardant Crosslinking Polyethylene Compound for Low Voltage Insulation

PTEKNP530 / 129610

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.