MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® BS V0 Nylon 6, Nucleated, Flame Retardant, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Nucleated; Nylon 6, Unreinforced, Flame Retardant

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Flame Retardant; Nucleating Agent

Features: Flame Retardant; Nucleated

Uses: Appliance Components; Automotive Applications; Automotive Electronics; Connectors; Electrical/Electronic Applications; Lighting Applications; Tubing; Wire & Cable Applications

RoSH Compliance: RoSH Compliant

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Water Absorption 2.5 %2.5 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 8.0 %8.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.3 MPa10200 psiISO 527-2
Tensile Strength, Yield 90.3 MPa13100 psiISO 527-2
Elongation at Break 4.0 %4.0 %ISO 527-2
Elongation at Yield 3.0 %3.0 %ISO 527-2
Tensile Modulus 3.70 GPa537 ksiISO 527-1
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.294 J/cm²1.40 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Dielectric Constant  3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 31.9 kV/mm810 kV/inIEC 60243-1
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.2 µm/m-°C39.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
Melting Point 222 °C432 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 120 °C248 °FLong Term; ISO 2578
 180 °C356 °FShort Term
Deflection Temperature at 0.46 MPa (66 psi) 170 °C338 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FUnannealed; ISO 75-2/A
Minimum Service Temperature, Air 100 °C212 °FLong Term; ISO 2578
Flammability, UL94  V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
IEC 60695-11-10,-20
 V-0
@Thickness 3.30 mm
V-0
@Thickness 0.130 in
IEC 60695-11-10,-20
Oxygen Index 32 %32 %ISO 4589-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM440 / 307799

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.