MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexBond™ EA9833.1 BMI Adhesive Film
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: Description: HexBond™ EA9833.1 50MIL is a 180°C/356°F cure modified bismaleimide foaming core splice adhesive.

Features:

  • High service temperature
  • Expansion: 100% to 150%
  • Storage life: 1 year minimum at or below -18°C/0°F + 3 weeks at room temperature (= 25°C/73°F)
Applications: Core splice bonding; Sandwich construction

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  6.00 MPa
@Temperature 210 °C
870 psi
@Temperature 410 °F
Tube, after Wet ageing: 1000 hours at 70°C/158°F and 85% relative humidity; EN 2667-2
 10.0 MPa
@Temperature 210 °C
1450 psi
@Temperature 410 °F
Tube; EN 2667-2
 10.5 MPa
@Temperature 149 °C
1520 psi
@Temperature 300 °F
Tube; EN 2667-2
 11.0 MPa
@Temperature 149 °C
1600 psi
@Temperature 300 °F
Tube, after Wet ageing: 1000 hours at 70°C/158°F and 85% relative humidity; EN 2667-2
 12.5 MPa
@Temperature 22.8 °C
1810 psi
@Temperature 73.0 °F
Tube; EN 2667-2
 14.5 MPa
@Temperature -55.0 °C
2100 psi
@Temperature -67.0 °F
Tube; EN 2667-2
 14.5 MPa
@Temperature 22.8 °C
2100 psi
@Temperature 73.0 °F
Tube, after Wet ageing: 1000 hours at 70°C/158°F and 85% relative humidity; EN 2667-2
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 280 °C536 °FWet ageing: 1000 hours at 70°C/158°F and 85% relative humidity
 293 °C559 °F
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9264 / 322420

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.