MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik 425 Acrylic Latex
Categories: Polymer; Thermoset

Material Notes: Bostik® 425 Multi-Purpose Acrylic Latex Admixture is a high solids acrylic emulsion designed to improve the performance of Bostik Ceramic Tile Grout, Bostik Dry Tile Grout, Bostik Tile-Mate™ Thin Set Mortars, Bostik Single Flex FS™ (Fast Set) Mortar and jobsite prepared mortar beds.

Product Use:

  • Controls hydration rate (curing) of cement mortars and grouts
  • Use with thin set mortars to provide adhesion to non-masonry substrates such as plywood, waterproofing and crack isolation membranes and porcelain tile
  • Use with cement based tile grouts. Helps to ensure consistent cure results and better color development
  • Improve water resistance of grouts, thin sets and mud beds
  • Improve flexural and compressive strengths
  • Helps prevent cracking grout in wood framed Structures
  • Use 425 Multi-Purpose Acrylic Latex Admixture to prepare bond coats
  • Use in jobsite prepared mortar “mud” beds

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 3.0 %50% relative humidity
 4.0 %Immersion to dry
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 400 psi
@Time 605000 sec
Ceramic Mosaic Tile
 400 psi
@Time 605000 sec
Glazed Wall Tile
 400 psi
@Time 605000 sec
Quarry to Wood
 4000 psi
@Time 605000 sec
With Ceramic Tile Grout
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hourInitial set at 70°f
Shelf Life 12.0 Month
@Temperature 1.11 - 37.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Overview of materials for PVC/Acrylic Alloy
BASF Basotect® G+ Foam
Bostik NeverSeal™ Grout
Bostik EzPoxy™ Epoxy Mortar & Grout

PBOSTK009 / 191545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.