MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Oxford Polymers 30GF 30% Glass Fiber Filled Polycarbonate for Injection Molding
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: 30% Glass Fiber Filled Polycarbonate for Injection Molding

Information provided by Oxford Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Filler Content 30 %30 %
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 131 MPa19000 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Tensile Modulus 8.62 GPa1250 ksiASTM D638
Flexural Strength 159 MPa23000 psiASTM D790
Flexural Modulus 7.58 GPa1100 ksiASTM D790
Compressive Strength 124 MPa18000 psiASTM D695
Izod Impact, Notched 1.07 J/cm
@Temperature 23.0 °C
2.00 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C305 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 293 °C560 °F
Back Pressure 103 MPa15000 psiMold pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy
Arkema Kynar® 705 PVDF
Syensqo (Solvay Specialty Polymers) Radel® R-5900 Polyphenylsulfone (PPSU)
PTS Tristar® PC-30GF 30% Glass Reinforced Polycarbonate With Release

POX29 / 55878

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.