MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
Categories: Polymer; Thermoplastic; ABS Polymer; PC/ABS + Stainless Steel; Polycarbonate/ABS Alloy, Antistat/Conductive; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10000 psiASTM D 638
Elongation at Break 3.0 %ASTM D 638
Tensile Modulus 550 ksiASTM D 638
Flexural Strength 17700 psiASTM D 790
Flexural Modulus 590 ksiASTM D 790
Izod Impact, Notched 1.20 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 9.70 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 100 ohmESD STM11.11
Surface Resistivity per Square <= 1000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 62 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 64 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 67 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 71 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 74 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 76 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °FASTM D 648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 470 - 525 °F
Mold Temperature 125 - 200 °F
Drying Temperature 200 °F
@Time 14400 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 2561 FR UV Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - UV Stabilized
RTP Company EMI 362 UV BLACK Polycarbonate (PC); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company ESD 187 Polypropylene (PP), Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PQZRA36591 / 206029

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.