MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolon® 265 PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: PVC Copolymer Blending Resin

F-265 is a fine particle size polyvinyl chloride vinyl acetate copolymer plastisol blending resin. The product has been designed for use in application where rapid gelation and fusion is a requirement, due to low processing temperatures. When used in combination with copolymer dispersion resin, F-265 has been successfully used in carpet backing, automotive sealants and underbody coatings as well as walk-off mats.

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³ASTM D1895
Volatiles 0.30 %0.30 %ASTM D3030
Particle Size 35 µm35 µmAverage; Coulter Counter LS230
Particle Mesh Size 40 Mesh40 Mesh100% thru; ASTM D1921B
 270 Mesh270 Mesh97% thru; ASTM D1921B
Viscosity 0.85 cP0.85 cPInherent; ASTM D1243
Relative Viscosity 1.95 cP1.95 cPQC-10-104
Vinyl Acetate Content 5.0 %5.0 %QC-10-105
 
Descriptive Properties
K-Value63Fikentscher's Constant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Formosa Plastics Formolon® 10 PVC
Formosa Plastics Formolon® 186 PVC
Formosa Plastics Formolon® 24A PVC

PFPCPQ109 / 150341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.