MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds Mold Max® 14NV Low Viscosity Tin Cure Silicone Rubber Compounds
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Mold Max™ 14NV and 29NV are tin-catalyzed silicone rubbers that offer low viscosity, fast cure and long library life. Mold Max™ 14NV and 29NV do not require vacuum degassing. Mix ratio is 100A:10B by weight. Pot life is 40 minutes. Cure time of 14NV is 4 hours at room temperature, cure time of 29NV is 6 hours at room temperature. Mold Max™ 14NV and 29NV will reproduce the finest detail and are suitable for a variety of industrial and art related applications including making molds for reproducing prototypes, furniture, sculpture and architectural elements. Cure time can be reduced with Accel-T™ cure accelerator. Mold Max™ 14NV and 29NV can be used to cast a variety of materials including wax, gypsum, low melt alloys/metals and urethane, epoxy or polyester resins. Important; Do not cast concrete into rubber molds made with this product. Concrete will not cure properly and inhibition will result. Important; you must weigh Part A & B components using a gram scale to be successful with Mold Max™ 14NV and 29NV.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D-1475
Viscosity 7500 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0020 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 14ASTM D-2240
Tensile Strength 490 psiASTM D-412
Elongation at Break 600 %ASTM D-412
100% Modulus 35.0 psiASTM D-412
Tear Strength 87.0 pliDie B; ASTM D-624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.83e+13 ohm-cmASTM D257-14
Surface Resistance 8.29e+11 ohmASTM D257-14
Dielectric Constant 3.29
@Frequency 100 Hz
ASTM D150-18
Dielectric Strength 330 V/milASTM D149-20
Dissipation Factor 0.0050
@Frequency 100 Hz
ASTM D150-18
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 205 °C
Minimum Service Temperature, Air -53.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
Pot Life 40.0 minASTM D-2471
 
Descriptive Properties
ColorWhite
Mix Ratio100A:10Bby weight
Specific Volume24.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN098 / 296799

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.