MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 201 C Nylon 11 (PA); Glass Fiber - 89% Renewable Resource Content
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11 with 10% Glass Fiber Filler

Material Notes: Renewable Resource Content calculated based on % of total compound weight.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D 792
Additive Loading 10 %Primary Additive
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D 785
Tensile Strength at Break 9000 psiASTM D 638
Elongation at Break 7.0 - 8.0 %ASTM D 638
Tensile Modulus 400 ksiASTM D 638
Flexural Strength 12000 psiASTM D 790
Flexural Modulus 350 ksiASTM D 790
Izod Impact, Notched 1.10 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 11.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 435 - 550 °F
Mold Temperature 100 - 150 °F
Drying Temperature 175 °F
@Time 14400 sec
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® MB 3000 NAT Nylon 11, Sheathing Grade
Arkema Rilsan® BZM 30 O TL PA11-GF30
Clariant Renol PA113G30TF15S2 Nylon 66, 30% Glass Fiber, Teflon and Silicone Lubricated
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled

PQZUA1202 / 134651

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.