MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Techmer ES HiFill FR® PA6 FR-N IM
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Impact Grade; Nylon 6, Unreinforced, Flame Retardant

Material Notes: Availability: North America

Forms: Pellets

Additive: Heat Stabilizer, Impact Modifier and Lubricant

Features: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated

Appearance: Red

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
Water Absorption 1.5 %
@Time 86400 sec
1.5 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.013 cm/cm
@Thickness 3.17 mm
0.013 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 50.3 MPa7300 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Flexural Strength 65.5 MPa9500 psiASTM D790
Flexural Modulus 1.72 GPa250 ksiASTM D790
Izod Impact, Notched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cmASTM D257
Dielectric Strength 16.5 kV/mm420 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 99.0 µm/m-°C55.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 166 °C330 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C125 °FUnannealed; ASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® HN-1064IA PC, Unreinforced FR
Westlake Plastics Radel® R 5500 Polyphenylsulfone
SEKISUI SPI KYDEX® 410 ABS/PVC
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Lotte Advanced Materials Infino® NH-1001T PC/ABS, Unreinforced FR

PTPC0663 / 136601

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.