Composed of finely dispersed EPDM in PP with dynamic complete cross-linking with organic peroxide. Features: - Excellent weather resistance and chemical resistance
- Low density
- Highly recyclable, and there is very little decline in properties even if it is reused
- Excellent heat resistance and excellent extrusion and intrusion formability
Information provided by Nishida Art Specialty Composite America Inc. |