Data provided by the manufacturer, Exxon Chemical. A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. It can be drawn down to less than 1.0 mil in the blown film process. Applications: Food packaging (bread bags, baked goods, light duty produce bags, etc.); Frozen food packaging; Textile goods packaging; Rack and counter bags where good heat sealability and clarity are required. Data for film properties below based on 1.25 mil film. |
Vinyl Acetate; Exxon Chemical Company |