MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® MP 5471 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP 5471 is a clear, two part unfilled electronics grade epoxy resin system. It was designed for applications where fast cure and excellent high temperature thermal stability is required. It cures very quickly at room temperatures to a tough, rigid polymer. It has good wetting and adhesion to most surfaces and has a free-flowing viscosity. It has excellent thermal stability and very good resistance to water, acids and bases and most organic solvents.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccpart B
 1.16 g/cc1.16 g/ccpart A
 1.16 g/cc1.16 g/ccmixed
Viscosity 1000 cP1000 cPpart A
 1100 cP1100 cPmixed
 10000 cP10000 cPpart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585instantaneous
Tensile Strength 58.6 MPa8500 psi
Elongation at Break 3.0 - 4.0 %3.0 - 4.0 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 8.30e+14 ohm-cm
@Temperature 25.0 °C
>= 8.30e+14 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 3.5
@Frequency 100 Hz,
Temperature 25.0 °C
3.5
@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 16.3 kV/mm415 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 1.00 - 1.25 min1.00 - 1.25 min5 grams
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Color / appearanceclear
Mix Ratio10:1 by volume (Part A to B)
 9.5:1 by weight (Part A to B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9096 / 233463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.