MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addocat® 5073 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Addocat 5073 is a heat latent catalyst for polyurethane mixtures based polyol and isocyanates (MDI). The mixtures are used as adhesives for Baynat with other materials. A processing temperature of approx. 60 °C is re-commended so as to activate the catalyst in the adhesive layer and in order to achieve proper adhesion / bonding. As Addocat 5073 hardly shows any discoloration effects neither in respect of PVC or other plastics, its use may be recommended for systems for PUR carpet backings as well as PVC back foaming.

Function: Heat latent catalyst for polyurethane adhesive mixtures, catalyst for PUR carpet backings and PVC back foaming.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Water Absorption <= 0.50 %<= 0.50 %
Viscosity 16 cP16 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 170 °C338 °FInitial
Pour Point -43.3 °C-46.0 °F
Flash Point 100 °C212 °FASTM D93, DIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Amine number152-172 mg HCl/g
Appearanceclear, colorless to pale yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8191 / 208584

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.