MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Opibent® 541 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Optibent® 541 is used as an additive for plasters to improve workability and gives setting retarding. Optibent® 541 is based on a white activated layer silicate and gives an improvement in processing and workability of plasters. Simultaneously, setting retarding is achieved and the incorporation of water into the dry plaster powder is improved. Optibent 541® gives extension of processing time and more open time for coat finishing, especially in white cement containing systems.

Applications:

  • Top Coats
  • Reinforcement Plasters
  • White Cement containing Products

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 - 0.750 g/cc
Brightness 70 %Elrepho R 457
pH 9.0 - 122% solution
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 0.000 - 40.0 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 12 %
 
Descriptive Properties
Color/Formwhite free flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Opibent® 1008 Layered Silicate
BYK Necowel FLE 55N Clay Additive
BYK Nanothix® B1490 Phylosilicate
BYK Mineral Colloid® MO Clay Additive
BYK Mineral Colloid® BP Bentonite

PBYK079 / 185076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.