MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ XP XP 8656MK Film Grade Hexene LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Exceed™ XP 8656MK is an eXtreme Performance ethylene 1-hexene copolymer that offers step-out toughness, high flex-crack resistance and increased output with excellent bubble stability for a range of blown film applications. TnPP is not intentionally added to 8656MK. 

Availability:  Africa & Middle East, Europe, North America, Asia Pacific, Latin America. 

Additive:  Exceed XP 86456MK:  antiblock: 5000 ppm, slip: 1000ppm;  processing aid: yes; thermal stabilizer: yes. 

Applications:  Agriculture film, construction liners,  liquid packaging, blown silage, flexible packaging.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.916 g/ccASTM D1505
Melt Flow 0.50 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1300 psiASTM D882
Film Tensile Strength at Yield, TD 1200 psiASTM D882
Film Elongation at Break, MD 280 %ASTM D882
Film Elongation at Break, TD 630 %ASTM D882
Puncture Energy 24.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 680 gASTM D1922
Elmendorf Tear Strength TD 680 gASTM D1922
Dart Drop Test 660 gASTM D1709
Film Tensile Strength at Break, MD 10000 psiASTM D882
Film Tensile Strength at Break, TD 7300 psiASTM D882
1% Secant Modulus, MD 26000 psiASTM D882
1% Secant Modulus, TD 28000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 249 °FPeak; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze >= 30 %ASTM D1003
Gloss 18 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ XP XP 8784MK Film Grade Hexene LLDPE
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
ExxonMobil Exceed™ XP XP 8358MJ Film Grade Hexene LLDPE
ExxonMobil Exceed™ XP XP 6026MQ Film Grade Hexene LLDPE
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin

PEX98822 / 238207

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.