MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® XE 4074 nat Nylon 6/12, Glass Bead, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass/Mineral Filler

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Glass Bead

Features: Food Contact Acceptable; Hydrolysis Resistant

Uses: Consumer Applications; Industrial Applications

Agency Ratings: ACS; DVGW W270; EU Food Contact; FDA Food Contact; KTW; NSF STD-61; WRAS

Appearance: Natural Color

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183
Water Absorption 0.50 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 1.1 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7250 psiISO 527-2
Elongation at Break 10 %ISO 527-2
Tensile Modulus 435000 psiISO 527-1
Charpy Impact Unnotched 19.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 29.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 1.90 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 1.90 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGRIM251 / 307610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.