MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Northstar Polymers MPP-A50A High Performance Polyether
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system exhibit fine resolution of mold details, good performance in wet environments and good resistance to ultraviolet light. This combination of features makes elastomers molded from MPP-A50A perfect for applications including patterns designed to transfer an image to wet surfaces including concrete and many custom applications.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ASTM D2240
Tensile Strength 2.14 MPa311 psiASTM D412
Elongation at Break 158 %158 %ASTM D412
100% Modulus 1.45 MPa
@Strain 100 %
211 psi
@Strain 100 %
ASTM D412
Tear Strength 1.21 kN/m6.90 pliSplit; ASTM D624
 11.7 kN/m67.0 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 5.45.4ASTM D4060
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 - 32.2 °C70.0 - 90.0 °FPrepolymer Temperature
 21.1 - 32.2 °C70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 21.1 - 32.2 °C70.0 - 90.0 °F
Cure Time  120 - 180 min
@Temperature 25.0 °C
2.00 - 3.00 hour
@Temperature 77.0 °F
De-mold Time
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Complete Cure Cycle
Pot Life 8.00 - 10.0 min8.00 - 10.0 min
 
Descriptive Properties
Curing AgentPBA-064
PrepolymerMPN-023
Weight Ratio1:2.799Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
Stratasys® FLX95050-DM Rubber-Like Digital Material
Northstar Polymers MPA-A30B Mold-Making Resin
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer

PNORTH821 / 162537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.