MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes:

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Moisture Absorption at Equilibrium 0.90 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 3.20 mm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ISO 2039
Tensile Strength at Break 113 MPaISO 527-1/-2
Elongation at Break 2.3 %ISO 527-1/-2
Tensile Modulus 8700 MPaISO 527-1/-2
Flexural Strength 170 MPaISO 178
Flexural Modulus 8200 MPaISO 178
Charpy Impact Unnotched 50.0 kJ/m²ISO 179-1
Charpy Impact, Notched 11.0 kJ/m²ISO 179-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CISO 11359-2
Flammability, UL94 V-0
@Thickness 0.750 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® C3 GF 60 1 black (4353) PA66 + PA6, Dry, 60% Glass Filled
Mitsubishi Chemical Advanced Materials Nylatron® 101 PA66 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Mitsubishi Chemical Advanced Materials Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
Envalior Akulon® Diablo HT-HG0 (K-X07029) PA66+PA6-GF50, Dry, 50% Glass Filled, Heat Stabilized

PUNITIK870 / 177890

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.