MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics ZTA Mac-ZTAA20W Technical Ceramic
Categories: Ceramic

Material Notes: Alumina-based material with mechanical properties enhanced by the addition of yttria partially-stabilised zirconia.

Applications:

  • Special ballistic applications
  • Pump and valve components for chemical processing duties where toughness and strength are required, together with resistance to wear and corrosion at elevated temperatures

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.32 g/ccfired
Porosity 0.00 %fully dense, nominal
Grain Size 2.0 µm
 430 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 350 GPaASTM C623 Mod
Poissons Ratio 0.24ASTM C623 Mod
Shear Modulus 145 GPaASTM C623 Mod
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+12 ohm-cm
@Temperature 100 °C
ASTM D150& D257 Mod
Dielectric Constant 12.5
@Frequency 1e+6 Hz
K'; ASTM D150 & D257 Mod
Dielectric Strength 85.3 kV/mmdc; ASTM D3755 Mod
Dissipation Factor 0.010
@Frequency 1000 Hz
ASTM D150& D257 Mod
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.30 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 20.0 W/m-Kcalculated
 
Component Elements PropertiesOriginal ValueComments
Al2O3 80 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics ZTA Zirconia Toughened Alumina
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
Astro Met ZTA 96 Zirconia Toughened Alumina
CoorsTek Zirconia-Toughened Alumina, ZTA
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide

CMORF8054 / 203531

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.