MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aurora Plastics TufFill™ 5000-SN4 PP, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Application: A No Bloom, UL 94 V-0 Polypropylene Compound TufFill™ 5000SN series is a specially engineered, low bloom, flame retardant polypropylene compound designed with halogen based technology. TufFill™ 5000SN series exhibits a balance of high flexural modulus and good impact. It is designed for extrusion applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 29.6 MPa>= 4300 psiASTM D638
Elongation at Break >= 100 %>= 100 %ASTM D638
Flexural Modulus 3.59 GPa521 ksitangent; ASTM D790
Flexural Modulus, 1% Secant 2830 MPa410000 psiASTM D790
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²ASTM D256
Dart Drop Total Energy 8.54 J/cm0.0160 ft-lb/milASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 126.5 °C
@Thickness 3213 mm
259.7 °F
@Thickness 126.5 in
0.125 in.; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.1 °C
@Thickness 3.17 mm
153 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Oxygen Index >= 25 %>= 25 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 210 °C380 - 410 °FProfile
 210 °C410 °FStock

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® QD 813 Y001 WOD Flame Retardant Polypropylene
Celanese SO.F.TER Polifor® QD 813 30% Glass Fiber Reinforced Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0-EP Mineral Filled Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0 EPWOD Flame Retardant Polypropylene
Celanese SO.F.TER Polifor® 5000/V0-AF-EP Self Extinguishing Polypropylene Copolymer, Flame Resistant

PSEPN008 / 179012

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.