Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Medium Gloss Uses: Automotive Interior Parts; Knobs Automotive Specifications: GM GMP.PVC.035 Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |