MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax CA 12 A Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax CA 12 A is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’ s proprietary Catalloy process technology. It is suitable for industrial applications where a combination of good processability and excellent softness is required. Hifax CA 12 A exhibits low stiffness, low hardness and good impact resistance. The material shows high compatibility to other polyolefins as well as to other soft plastics. Hifax CA 12 A is cross linkable. The grade is available in natural pellet form. Applications: Bottles for Industrial Use, Interior Automotive Applications, Polymer Modifier, TPO Foils and Skins, Wire & Cable.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccmethod A; ISO 1183-1
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 36ISO 868
Tensile Strength at Break 13.0 MPaISO 527-1,-2
Tensile Strength, Yield 9.00 MPaISO 527-1,-2
Elongation at Break 550 %ISO 527-1,-2
Elongation at Yield 35 %ISO 527-1,-2
Flexural Modulus 330 MPaISO 178
Charpy Impact, Notched 100 kJ/m²
@Temperature -20.0 °C
ISO 179
 100 kJ/m²
@Temperature -40.0 °C
ISO 179
 NB
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 78.0 °CA50; ISO 306
 
Descriptive Properties
Processing MethodCalendaring, Compounding, Extrusion Blow Molding, Extrusion Flat-die, Sheet, Wire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7174 / 218811

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.