MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Orbilan ORBILAN® PE 1000 UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general machine and plant construction, transport and electroplate techniques, bunker and silo linings to the manufacture of fenders and sluices for hydraulic architecture.

Information provided by the manufacturer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccISO 1183
Molecular Weight >= 5.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Ball Indentation Hardness 38.0 MPaISO 2039
Tensile Strength, Yield >= 17.0 MPaISO 527-1
Elongation at Break >= 350 %ISO 527-1
Elongation at Yield <= 15 %ISO 527-1
Modulus of Elasticity >= 0.650 GPaISO 527-1
Charpy Impact, Notched >= 20.0 J/cm²ISO 179
Coefficient of Friction 0.14DIN 53 375
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmDIN 53 482
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 - 200 µm/m-°C
@Temperature 20.0 - 80.0 °C
DIN 53 752-A
Thermal Conductivity 0.410 W/m-K
Maximum Service Temperature, Air 80.0 °Ccontinuous
Minimum Service Temperature, Air -60.0 °Ccontinuous
 
Descriptive Properties
Attrition100Sand-Slurry procedure
Water Absorption< 0.01 mg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000
Hippe PE 1000 Polyethylene
Omnia Plastica PE 1000 - Polyethylene 1000
Chi Mei Wonderloy® PC-345 PC/ABS Alloy
Bakelite® PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength

PORBIL00 / 55702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.