MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Loxim 110 01V0 Polycarbonate, 10% Glass Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes:

Information provided by Loxim Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Filler Content 10 %
Linear Mold Shrinkage 0.0030 cm/cmASTM D1299
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 - 80.0 MPaASTM D683
Elongation at Break 10 - 20 %ASTM D638
Tensile Modulus 3500 MPaASTM D638
Flexural Modulus 3500 MPaASTM D790
Izod Impact, Notched 80.0 - 90.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 - 145 °CASTM D1525, HDT Method B
Flammability, UL94 V-0
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kotec Carbotex KGN-10MRA Polycarbonate, Flame Retardant, 10% Glass Fiber Reinforced
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced

PLOXIM023 / 121357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.