MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 9608XD HDPE Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: This HDPE is tailored for applications that require:
  • Very low gel levels
  • Very "clear" film
  • Excellent drawdown
  • Enhanced stiffness
  • Excellent WVTR for a chill cast film
  • Excellent Processibility
Typical Cast Film Applications:
  • Coextrusions
  • Overwrap
  • Food packaging
  • Moisture sensitive packaging
Property data based on 1.25 mil cast film.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.962 g/ccASTM D1505
Water Vapor Transmission 5.00 g/m²/dayASTM F1249
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 870 %ASTM D882
Film Elongation at Break, TD 790 %ASTM D882
Elmendorf Tear Strength, MD 35.0 g/milASTM D1922
Elmendorf Tear Strength, TD 100 g/milASTM D1922
Dart Drop 35.0 g/milASTM D1709
Film Tensile Strength at Break, MD 29.0 MPaASTM D882
Film Tensile Strength at Break, TD 23.0 MPaASTM D882
1% Secant Modulus, MD 110000 psiASTM D882
1% Secant Modulus, TD 122000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 11 %ASTM D1003
Gloss 120 %60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB3450 HDPE for Film Extrusion
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Borealis Borstar® FB1460 HDPE for Film
Americas Styrenics STYRON® 484 High Impact Polystyrene

PCHEVF100 / 86300

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.