MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 4007 Polyphthalamide (PPA), Glass Fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/ccASTM D 792
Water Absorption 0.18 %
@Time 86400 sec
0.18 %
@Time 24.0 hour
ASTM D 570
Additive Loading 40 %40 %Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 125125ASTM D 785
Tensile Strength at Break 221 MPa32000 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 14.8 GPa2150 ksiASTM D 638
Flexural Strength 317 MPa46000 psiASTM D 790
Flexural Modulus 13.8 GPa2000 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.20 mm
2.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 6.41 J/cm
@Thickness 3.20 mm
12.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 5.8
@Frequency 1e+6 Hz
5.8
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 19.7 kV/mm500 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°FE 831
Deflection Temperature at 1.8 MPa (264 psi) 279 °C535 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 302 - 329 °C575 - 625 °F
Mold Temperature 135 - 163 °C275 - 325 °F
Drying Temperature 107 °C
@Time 14400 - 21600 sec
225 °F
@Time 4.00 - 6.00 hour
Moisture Content 0.050 %0.050 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 4008 Polyphthalamide (PPA), Glass Fiber
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA
RTP Company RTP 4005.3 HS Polyphthalamide (PPA), Glass Fiber - Heat Stabilized
RTP Company RTP 4003 Polyphthalamide (PPA), Glass Fiber
RTP Company RTP 4009 Polyphthalamide (PPA), Glass Fiber

PQZWA3201 / 91584

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.