MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvax® 3128-1 Ethylene Vinyl Acetate
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

ELVAX® 3128-1 EVA Resin complies with Food and Drug Administration Regulation 21 CFR 177.1350(a)(1) - - Ethylene-vinyl acetate copolymers, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (b)(1) of the Regulation.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792, ISO 1183
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 83.0 °CFreezing Point; ASTM D3418, ISO 3146
 99.0 °CASTM D3418, ISO 3146
Vicat Softening Point 77.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 235 °C
Feed Temperature 135 °CBlown Film Coextrusion
 135 °CCast Film/Sheet Processing
Zone 2 160 °CBlown Film Coextrusion
 160 °CCast Film/Sheet Processing
Zone 3 185 °CBlown Film Coextrusion
 185 °CCast Film/Sheet Processing
Zone 4 185 °CBlown Film Coextrusion
 210 °CCast Film/Sheet Processing
Zone 5 185 °CBlown Film Coextrusion
 210 °CCast Film/Sheet Processing
Adapter Temperature 185 °CBlown Film Coextrusion
 210 °CCast Film/Sheet Processing
Die Temperature 185 °CBlown Film Coextrusion
 210 °CCast Film/Sheet Processing
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvax® 440 Ethylene Vinyl Acetate
Dow Elvax® 3175LGA Ethylene Vinyl Acetate
Dow Elvax® 3169Z Ethylene Vinyl Acetate
Dow Elvax® 3155 Ethylene Vinyl Acetate
Dow Elvax® 3190A Ethylene Vinyl Acetate

PDTA4943 / 170383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.