MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Hysol EA 9258.1 Primer
Categories: Polymer; Thermoset

Material Notes: Waterborne, corrosion-inhibiting primer, designed to provide enhanced toughness and high temperature performance where continuous exposures up to 350°F / 177°C are required. Meets SCAQMD Rule 1124.
    Applications:
  • Sprayable
  • Low Viscosity Wet Lay-up
  • Metal and Honeycomb Bonding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 5.00 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7.00 MPaFlatwise
Adhesive Bond Strength 19.0 MPa
@Temperature 177 °C
Lap Shear
 27.0 MPa
@Temperature -55.0 °C
Lap Shear
 33.0 MPa
@Temperature 22.0 °C
Lap Shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 177 °C
 
Descriptive Properties
Honeycomb Climbing Drum Peel, mN/m60at 25°C
Out-Time (days)30at 25°C
Primer Coverage, sq.m/L416at 8µm dry film thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9257 Primer

PHENK852 / 146857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.