Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight Additive: Lubricant, UV Stabilizer and Heat Stabilizer Features: Lubricated, Good UV Resistance and Heat Stabilized Information provided by TP Composites, Inc. |