MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method.

Application: Composition is intended to be processed into pressure pipes and connection elements for pipeline systems.

Information Provided by Kazanorgsintez

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 - 0.960 g/cc
@Temperature 23.0 °C
 0.956 - 0.962 g/cc
@Temperature 20.0 °C
Volatiles <= 0.035 %
Environmental Stress Crack Resistance >= 20 hour
@Temperature 80.0 °C
with initial wall stress 2 MPa (on pipe samples d32 mm SDR 11)
 >= 165 hour
@Temperature 80.0 °C
with initial wall stress 4.6 MPa (on pipe samples d110 mm SDR 11)
 >= 500 hour
@Temperature 80.0 °C
with initial wall stress 4.6 MPa (on pipe samples d160 mm SDR 11)
Carbon Black Loading 2.0 - 2.5 %
Melt Flow 0.029 - 0.070 g/10 min
@Load 2.16 kg,
Temperature 190 °C
±10%
 0.10 g/10 min
@Load 5.00 kg,
Temperature 190 °C
 5.0 - 7.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 21.0 MPa
Elongation at Break >= 500 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
@Time >=1200 sec
 
Descriptive Properties
Carbon Black Distribution TypeI-II
Stability at Constant Internal Pressure 20°C; hr2500with initial wall stress 11.6 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Formosa Plastics Formolene® HP4306 Pipe HDPE
CoorsTek Yttria Partially Stabilized Zirconia, YTZP, Sintered
LyondellBasell Hostalen CRP 100 S YELLOW High Density Polyethylene (HDPE), Pipe Grade
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite

PKAZAN009 / 127328

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.