MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.34 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 113
@Temperature 23.0 °C
ASTM D785
Tensile Strength, Yield 64.1 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 5070 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 103 MPa1.3 mm/min; ASTM D790
Flexural Modulus 4550 MPa1.3 mm/min; ASTM D790
Izod Impact, Notched 53.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Izod Impact, Unnotched 370 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 194 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 271 - 293 °C
Mold Temperature 82.2 - 135 °C
Drying Temperature 79.4 °C
Dry Time 4.00 hour
 
Descriptive Properties
AppearanceBlack
FeaturesHigh Specific Gravity
 Non-Toxic
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliance Components
 Automotive Applications
 Consumer Applications
 Handles
 Industrial Applications
 Knobs
 Medical/Healthcare Applications
 Metal Replacement
 Sporting Goods
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6)
Avient Gravi-Tech™ GRV-NY-050-CU-NAT Polyamide 6 (Nylon 6)
Avient Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6)
Avient Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6)

PH0POL1270 / 145839

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.