MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Lastilac AR-V0E ABS, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0045 - 0.0065 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8.00 MPa
@Temperature 90.0 °C
 15.0 MPa
@Temperature 60.0 °C
 35.0 MPa
@Temperature 23.0 °C
Elongation at Break 8.0 %
@Temperature 23.0 °C
 50 %
@Temperature 60.0 °C
 95 %
@Temperature 90.0 °C
Elongation at Yield 2.0 %
@Temperature 23.0 °C
 2.3 %
@Temperature 60.0 °C
 2.3 %
@Temperature 90.0 °C
Tensile Modulus 1500 MPa
@Temperature 90.0 °C
 1900 MPa
@Temperature 60.0 °C
 2300 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -20.0 °C
 50.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -20.0 °C
 7.00 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 350 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
Vicat Softening Point 95.0 °C
@Load 5.00 kg
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
Oxygen Index 28 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
Glow Wire Ignition Temperature 725 °C
@Thickness 2.00 mm
 850 °C
@Thickness 1.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 210 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 70.0 - 80.0 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Abifor® 7145/V0-UV Self Extinguishing ABS, Flame Resistant
LATI LASTILAC AR-V0 Acrylonitrile Butadiene Styrene (ABS) (UL94 V-0 5V)
LATI LASTILAC ARUV-V0 Acrylonitrile Butadiene Styrene (ABS) (UL94 V-0 5V)
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade
Celanese SO.F.TER Abifor® 6080/V0 Self Extinguishing ABS, Flame Resistant

PLATH9667 / 177363

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.