Vydyne R530J NT0724 is a natural, 30% glass filled, high flow, PA66 that is heat stabilized with an electrically neutral heat stabilizer. It is specially designed for electrical applications requiring high dielectric strength, low conductivity, and corrosion resistance.Information provided by Ascend Performance Materials. |