MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Glastic SG-200 Industrial Lift Magnet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature NEMA GPO-1 products. It is also a superior replacement material for epoxy-bonded mica in layer insulation applications. SG-200 features the following:
  • Extremely strong
  • Excellent retention of properties at elevated temperatures
  • Ideal for high temperature applications
  • Easily fabricated
  • Asbestos-Free

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D-792
Water Absorption 0.30 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 12500 psiASTM D-638
Tensile Modulus 1.70e+6 psiASTM D-638
Flexural Strength 29000 psiASTM D-790
Compressive Strength 36000 psiASTM D-695
Shear Strength 11100 psiASTM D-732
Izod Impact, Notched 12.0 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.45e+14 ohmASTM D-257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D-150
 4.6
@Frequency 60 Hz
ASTM D-150
Dielectric Strength 19.6 kV/mmPerpendicular S/T in Air; ASTM D-149
 24.6 kV/mmPerpendicular S/T in Oil; ASTM D-149
Dissipation Factor 0.013
@Frequency 1e+6 Hz
ASTM D-150
 0.037
@Frequency 60 Hz
ASTM D-150
Arc Resistance 120 secASTM D-495
 180 secPost-cured; ASTM D-495
Comparative Tracking Index >= 500 VUL 746A
Hot Wire Ignition, HWI 35 sec
@Thickness 0.711 mm
UL 746A
 39 sec
@Thickness 1.47 mm
UL 746A
High Amp Arc Ignition, HAI >= 200 arcs#Exposure; UL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
ASTM D-696
Thermal Conductivity 0.250 W/m-KASTM C-177
UL RTI, Electrical 210 °CUL 746B
UL RTI, Mechanical without Impact 210 °CUL 746B
Flammability, UL94 HB
Oxygen Index 21.8 %ASTM D-2863
 
Descriptive Properties
Electric Strength kV, ASTM D14950Parallel S/S in Oil
Standard ColorNatural/Tan
UL Recognition File NumberE81928

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
Röchling Glastic Laminates/Shapes 1580 Polyester Laminate
A. Schulman Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC

PGLASW4 / 41938

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.