Notes: Monprene SP-13064 is a high performance thermoplastic elastomer designed for a variety of consumer applications. Monprene SP-13064 is a translucent, medium hardness, low density, high flow grade suited for extrusion and injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Medium Flow; Low Density; Low Specific Gravity; Medium Hardness; Without Fillers Uses: Consumer Applications; Gaskets; Handles; Kitchenware; Sporting Goods; Tubing; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex |