MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Avient Maxxam™ FR PP 401 CS Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.928 g/cc0.928 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.011 - 0.020 cm/cm0.011 - 0.020 in/inASTM D955
Melt Flow 6.4 - 9.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.4 - 9.1 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.4 MPa4700 psiType I, 51 mm/min; ASTM D638
Elongation at Break 290 %290 %Type I, 51 mm/min; ASTM D638
Flexural Modulus 1.38 GPa200 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.00 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 3.18 mm
203 °F
@Thickness 0.125 in
Annealed; ASTM D648
UL RTI, Mechanical without Impact 105 °C221 °FUL 746
Flammability, UL94 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
All colors; Internal Method
Oxygen Index 27 %
@Thickness 3.18 mm
27 %
@Thickness 0.125 in
ASTM D2863
 
Descriptive Properties
FeaturesFlame Retardant
 Medium Flow
FormsPellets
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical AF-325 ABS Resin
Covestro Makrolon® FR 7087 Polycarbonate
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade
Avient Maxxam™ FR PP 402 Polypropylene

PH1PN9134 / 102970

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.