MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo Pelprene™ P-70B Polyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyether Ester Elastomer

Material Notes: Key Feature: Pelprene P type

Pelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block copolymer consisting of an aromatic polyester as the hard segment and an aliphatic polyether as the soft one. It covers general purpose grades, being designed to have a balance of flexibility, heat & cold resistance, chemical resistance, and processability.

Information provided by Toyobo Co., Ltd

Key Words: Thermoplastic Elastomer; Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Moisture Absorption at Equilibrium 0.43 %25°C; 65%RH
Linear Mold Shrinkage 0.010 cm/cm
@Thickness 2.00 mm
Melt Flow 20 g/10 min
@Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96ASTM D2240
Hardness, Shore D 46ASTM D2240
Tensile Strength, Ultimate 12.0 MPaASTM D638
Elongation at Break 550 %ASTM D638
50% Modulus 0.0108 GPa
@Strain 50 %
ASMT D638
Flexural Modulus 0.108 GPaASTM D790
Compressive Modulus 0.00920 GPa10% Compression Modulus; ASTM D695
Resilience 71JIS K6301
Izod Impact, Notched NBASTM D256
Tear Strength 122 kN/mASTM D624
Taber Abrasion, mg/1000 Cycles 15CS-17 wheel; ASTM D1044
Compression Set 55 %
@Temperature 70.0 °C
70°C; 22 hrs; JIS K6301
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 6.00e+13 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mmJIS K2111
 
Thermal PropertiesOriginal ValueComments
CTE, linear 160 µm/m-°C
@Temperature 20.0 °C
TMA
Melting Point 200 °CDSC
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CASTM D648
Vicat Softening Point 170 °CASTM D1525
Brittleness Temperature -65.0 °CJIS K6301
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toyobo PELPRENE™ P55B Polyester TPE
Toyobo Pelprene™ S-1001 Polyester TPE
Toyobo Pelprene™ P-30B Polyester TPE
Celanese Hytrel® G3548 NC010 TPC-ET
Celanese Riteflex® 425 TPC, Unfilled

PTOY35 / 70707

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.