MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro DESMODUR® ML31106 + BAYTEC® XL AL905 (SD11-3) 95 A Polyurethane, MDI- Caprolactone
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccBAYTEC® XL AL905
 1.12 g/cc1.12 g/ccDESMODUR® ML31106
 1.18 g/cc1.18 g/cc
Viscosity 30 cP30 cPBAYTEC® XL AL905
 1200 cP1200 cPDESMODUR® ML3182
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595DIN 53505
 92
@Temperature 80.0 °C
92
@Temperature 176 °F
DIN 53505
 97
@Temperature -5.00 °C
97
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 50.0 MPa7250 psiDIN 53504
Tensile Stress at Strain 5.00 MPa
@Strain 10 %
725 psi
@Strain 10 %
DIN 53504
Elongation at Break 430 %430 %DIN 53504
100% Modulus 11.9 MPa
@Strain 100 %
1730 psi
@Strain 100 %
DIN 53504
200% Modulus 18.6 MPa
@Strain 200 %
2700 psi
@Strain 200 %
DIN 53504
300% Modulus 30.4 MPa
@Strain 300 %
4410 psi
@Strain 300 %
DIN 53504
Resilience 3636[%]; DIN 53512
Tear Strength 82.0 kN/m468 pliwith nick; ISO 34-1
 142 kN/m810 pliwithout nick; ISO 34-1
Abrasion 3535[mm3]; ISO 4649
Compression Set 23 %
@Temperature 70.0 °C,
Time 79200 sec
23 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FBAYTEC® XL AL905
 70.0 °C158 °FDESMODUR® ML31106
Mold Temperature 100 °C212 °F
Pot Life 2.00 min2.00 minwith SD11-3 catalyst
 3.00 min3.00 minwithout catalyst
 
Descriptive Properties
AppearancesolidDESMODUR® ML31106
 solidBAYTEC® XL AL905
Content0.08SD11-3 catalyst % / total (by weight), (catalyst at the head)
 10.4-10.8%NCO, DESMODUR® ML31106
 100Parts by weight of prepolymer
 11.1Parts by weight of BAYTEC® XL AL905

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® MLQ22165 + BAYTEC® L20 + BAYTEC® XL B (Catalyst SD11-2) 75 A Polyurethane, MDI- Caprolactone
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane
Covestro DESMODUR® TL535 + MOCA, 70 A Polyurethane, TDI- Caprolactone
Covestro DESMODUR® TL535 + BAYTEC® XL 1705, 80 A Polyurethane, TDI- Caprolactone
Covestro DESMODUR® ML3182 + BAYTEC® XL AL905 (SD11-3) 90 A Polyurethane, MDI- Caprolactone

PCOVEST0491 / 202274

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.